D6040-06 Standard Guide to Standard Test Methods for Unsintered Polytetrafluoroethylene (PTFE) Extruded Film or Tape

Published By Publication Date Number of Pages
ASTM 2006 3
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

1.1 This guide identifies test methods to use in evaluating unsintered extruded films or tapes manufactured from polytetrafluoroethylene.

1.2 The values stated in SI units as detailed in IEEE/ASTM SI 10, are to be regarded as standard.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Note 1This test method is equivalent to ISO 12086-2:2006 in the measurement of tensile properties, specific gravity, and dielectric constant. These are in ISO 12086-2:2006, sections 8.2.2, 10.6 and 8.1.1. It is not equivalent to ISO 12086-2:2006 in any other measurement or section..

PDF Catalog

PDF Pages PDF Title
1 Scope
Referenced Documents
Terminology
Test Specimens
Conditioning
2 Width
Thickness
Tensile Properties
Specific Gravity (Relative Density)
Residual Extrusion Aids or Other Volatile Components
Dielectric Constant
Volume Resistivity
Dielectric Breakdown Voltage
Unit Weight
3 Keywords