{"id":118531,"date":"2024-10-19T03:58:23","date_gmt":"2024-10-19T03:58:23","guid":{"rendered":"https:\/\/pdfstandards.shop\/product\/uncategorized\/astm-a355-2006\/"},"modified":"2024-10-24T22:41:15","modified_gmt":"2024-10-24T22:41:15","slug":"astm-a355-2006","status":"publish","type":"product","link":"https:\/\/pdfstandards.shop\/product\/publishers\/astm\/astm-a355-2006\/","title":{"rendered":"ASTM-A355 2006"},"content":{"rendered":"<\/p>\n
1.1 This specification covers alloy steel bars, suitable for surface hardening by nitriding, designated as Classes A, B, C, and D. Class A and Class D bars are general-purpose bars; Class B bars are free-machining bars; Class C bars contain 3.50 % nickel and are characterized by higher core strength. All classes are normally furnished in the hot-rolled, quenched, and tempered condition. However, centerless-ground or turned bars, in any of the classes, may be specified by the purchaser. Also, as-rolled, annealed, or unannealed bars suitable for forging may be purchased to this specification. When as-rolled, annealed, or unannealed bars are furnished, Sections 6, 10, and 11 are not applicable.<\/p>\n
1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.<\/p>\n
PDF Pages<\/th>\n | PDF Title<\/th>\n<\/tr>\n | ||||||
---|---|---|---|---|---|---|---|
1<\/td>\n | Scope Referenced Documents Ordering Information Process Discard Quenching and Tempering Microstructure Decarburization Heat Analysis <\/td>\n<\/tr>\n | ||||||
2<\/td>\n | Straightness Hardness Test Permissible Variations in Dimensions Length Workmanship, Finish, and Appearance General Requirements Keywords TABLE 1 TABLE 2 TABLE 3 TABLE 4 <\/td>\n<\/tr>\n<\/table>\n","protected":false},"excerpt":{"rendered":" A355-89(2006) Standard Specification for Steel Bars, Alloys, for Nitriding<\/b><\/p>\n |